MortarFlash™ | 40-Mil Non-Asphaltic Flashing
Technical Data
Features
- Available in 12″, 16, 18″, 24″, and 36″ x 75′ rolls
- Other sizes available upon request
- Tear resistant
- Will not drool when exposed to UV or heat
- Primer is not required; however, we recommend the use of a termination bar and a bead of sealant under the leading edge of the flashing
- When the use of prefabricated accessories is not feasible, MortarFlash™ Non-Asphaltic can be used to create inside and outside corners.
Technical Data
- UV Accelerated Weathering ASTM G154
- Mullen Burst ASTM D751 – 400 psi – 2760 kPa
- More than 90% strength retained after 2000 hours exposure
- Heat Resistance
- Short Exposure – 194°F. (90°C)
- Continuous Exposure – 160°F. (71°C)
- Melting Point – 230°F (110°C)
- Tensile Strength ASTM D751
- Machine Direction – 230 lbs. – 105 kg.
- Cross Direction – 210 lb. – 95 kg.
- Force Elongation 20%
Available Flashing Components
Recommended for use with MortarFlash Non-Asphaltic
- Termination Bars
- PVC – 1/8″ thick, UV stabilized
- Stainless steel – 16 gauge Type 304
- Stainless steel w/ lip – 16 gauge Type 304
- Drip Edge
- Stainless Steel – 28 gauge Type 304
- Kynar-coated galvanized steel – 24 gauge
- Cold-rolled copper – 24 gauge
- Inside/Outside Corners & End Dams
- Synthetic Rubber (SR)
- Thermoplastic Polyolefin (TPO)
- Metal Drip Edge Corners
- Pre-formed outside 90°
- Adjustable 325° to 22°
Sizes and Packaging
THICKNESS | ROLL HEIGHT | ROLL LENGTH | ROLLS/PALLET | SF/BOX | SF/PALLET |
0.040″ | 9″ | 75′ | 196 | 225 | 11,025 |
12″ | 147 | 225 | 11,025 | ||
16″ | 104 | 200 | 10,400 | ||
18″ | 98 | 225 | 11,025 | ||
20″ | 84 | 125 | 10,500 | ||
24″ | 84 | 150 | 12,600 | ||
36″ | 49 | 225 | 11,025 |